Engineering the ZnO/SiO2 Interface for tunable optoelectronic and charge transport properties in Core–Shell nanostructures

Document Type

Article

Publication Date

10-2026

Abstract

ZnO@SiO₂ (ZS) core-shell heterostructures were prepared through the sol-gel method. The physicochemical results confirm the formation of ZnO nanoparticles coated with SiO₂ by different shell thicknesses (8.2, 14.5, and 20.5 nm). Upon increasing the shell thickness, the crystallite size was reduced and the microstrain was enhanced, while the microstrain increased from 6 × 10−4 for ZnO to 13 × 10−4 for ZS₃; this can be attributed to the interfacial stress between the amorphous SiO₂ shell and the crystalline ZnO core. Additionally, the XPS confirms the formation of a Si-O-Zn bond with an oxygen vacancy in the heterostructure. The optical absorption redshifted from 365 nm for ZS0 to 369, 384, and 389 nm for ZS core-shell structures. The bandgap for ZnO is 3.17 eV; as the shell thickness increases, the bandgap decreases to 3.05, 2.94, and 2.84 eV, respectively. While the refractive index, extinction coefficient, and optical conductivity (spot) were enhanced upon increasing the shell thickness of SiO₂. Additionally, the presence of the SiO₂ shell effectively suppresses conduction losses by acting as an insulating barrier. However, thicker shells introduce more interfacial regions, which can slightly increase dielectric loss at lower frequencies, potentially impacting the overall performance of the ZnO@SiO₂ nanostructures in optoelectronic applications. Furthermore, a noticeable decrease in conductivity is observed for ZS1, ZS2, and ZS3, confirming the dominant insulating effect of the SiO₂ shell. These findings demonstrate that the optoelectronics features and electrical conductivity can be effectively tuned by controlling the SiO₂ shell thickness.

Share

COinS